TOPCon solar cell achieves 24.2% efficiency via new plasma-assisted atomic layer deposition tech

… the atomic scale. “This new technology is aimed to solve the … novel industrial tube-based PEALD technology with demonstrated commercial TOPCon cell … University, Chinese cell maker Tongwei, Singapore';s Institute of Materials …